Optical Windows with Anti-Reflection Coating

WBMA

Optical Windows with Anti-Reflection Coating
In stock
SKU
WBMA
These optical windows have high-quality and may be used when light is passed through the opposite side of the partition or in the vacuum chamber. Since the windows have anti-reflection coatings the transmittance is increased so they can be used as a window for laser irradiation windows and the observation of the sample.
custom product
Customize product
Filters
Enabled filters :
Remove all filters
Name Diameter φD Delivery Price Add to cart
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-30C03-10-IR1
30mm
6-12 weeks
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ30mm
Thickness t 3mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-15C02-10-IR2
15mm
6-12 weeks
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ15mm
Thickness t 2mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-20C03-10-IR2
20mm
6-12 weeks
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ20mm
Thickness t 3mm
i
Optical Window BK7 25.4mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-25.4C03-10-IR2
25.4mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ25.4mm
Thickness t 3mm
i
Optical Window BK7 40mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-40C04-10-IR2
40mm
6-12 weeks
£131.70
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ40mm
Thickness t 4mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-20C02-10-550
20mm
1 week
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ20mm
Thickness t 2mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-25C03-10-550
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ25mm
Thickness t 3mm
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-30C03-10-550
30mm
6-12 weeks
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ30mm
Thickness t 3mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-15C02-10-IR1
15mm
6-12 weeks
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ15mm
Thickness t 2mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-20C03-10-IR1
20mm
6-12 weeks
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ20mm
Thickness t 3mm
i
Optical Window BK7 25.4mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-25.4C03-10-IR1
25.4mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ25.4mm
Thickness t 3mm
i
Optical Window BK7 40mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-40C04-10-IR1
40mm
6-12 weeks
£131.70
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ40mm
Thickness t 4mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-15C03-10-IR2
15mm
1 week
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ15mm
Thickness t 3mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-25C02-10-IR2
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ25mm
Thickness t 2mm
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-30C02-10-IR2
30mm
1 week
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ30mm
Thickness t 2mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-15C02-10-550
15mm
1 week
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ15mm
Thickness t 2mm
i
Optical Window BK7 50mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-50C05-10-IR2
50mm
1 week
£181.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ50mm
Thickness t 5mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-20C03-10-550
20mm
1 week
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ20mm
Thickness t 3mm
i
Optical Window BK7 25.4mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-25.4C03-10-550
25.4mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ25.4mm
Thickness t 3mm
i
Optical Window BK7 40mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-40C04-10-550
40mm
1 week
£131.70
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ40mm
Thickness t 4mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-15C03-10-IR1
15mm
6-12 weeks
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ15mm
Thickness t 3mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-25C02-10-IR1
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ25mm
Thickness t 2mm
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-30C02-10-IR1
30mm
1 week
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ30mm
Thickness t 2mm
i
Optical Window BK7 50mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-50C05-10-IR1
50mm
1 week
£181.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ50mm
Thickness t 5mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-20C02-10-IR2
20mm
1 week
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ20mm
Thickness t 2mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-25C03-10-IR2
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ25mm
Thickness t 3mm
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 750 - 1550nm
WBMA-30C03-10-IR2
30mm
6-12 weeks
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 750 - 1550nm
Diameter φD φ30mm
Thickness t 3mm
i
Optical Window BK7 15mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-15C03-10-550
15mm
1 week
£57.60
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ15mm
Thickness t 3mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-25C02-10-550
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ25mm
Thickness t 2mm
i
Optical Window BK7 30mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-30C02-10-550
30mm
6-12 weeks
£90.50
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ30mm
Thickness t 2mm
i
Optical Window BK7 50mm Diameter Anti-reflection Coated 400 - 700nm
WBMA-50C05-10-550
50mm
in stock
£180.80
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 400 - 700nm
Diameter φD φ50mm
Thickness t 5mm
i
Optical Window BK7 20mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-20C02-10-IR1
20mm
6-12 weeks
£65.90
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ20mm
Thickness t 2mm
i
Optical Window BK7 25mm Diameter Anti-reflection Coated 633 - 1064nm
WBMA-25C03-10-IR1
25mm
6-12 weeks
£74.10
Material BK7
Surface flatness λ/10
Parallelism <5″
Coating Dielectric multi-layer coating
Incident angle
Laser Damage Threshold 4J/cm2
Surface Quality <br> (Scratch-Dig) 40-20
Wavelength range 633 - 1064nm
Diameter φD φ25mm
Thickness t 3mm

You must be logged in to ask questions

◦By anti-reflection coating with a dielectric multi-layer, it is reduced to less than 1% to 4% reflection loss of the glass surface.
◦Since we are using the high quality material, the image will not be distorted by the transmission of the glass, and the laser beam is not diffused.
◦When you insert an window perpendicular to the optical path of the laser, the angle of the transmitted beam will not be changed.

We detect that you are accessing the website from a different region. You will be redirected to a local version of OptoSigma.

Your requested the page :

UNITED KINGDOM

Redirection to :